ABS filament
A tough filament that softens from about 85°C and can be smoothed with acetone, but warps badly without an enclosed printer.
ABS (acrylonitrile butadiene styrene) is the plastic of LEGO bricks, car parts and phone cases. As a 3D printing filament it is tough and holds its shape in warm places, softening from about 85°C under load. That is well above the roughly 69°C a dashboard in the sun reached in a published parked-car study.
The price is a harder print. ABS warps, it gives off fumes and it needs an enclosed printer. Prusa calls its warping “significant”.
Why ABS needs an enclosed printer and fresh air
Prusa lists “requires printer enclosure” and “significant warping” side by side as ABS drawbacks. Its answer is a bed heated to at least 100°C and a printer inside an enclosure that holds a warmer ambient temperature.
| Setting | ABS |
|---|---|
| Nozzle temperature | 255°C (Prusa profile) |
| Bed temperature | 100°C, 80 to 110°C by part size (Prusa profile) |
| Enclosed printer | Needed |
| Drying | Only if damp: 80°C for 8 hours |
Without an enclosure, Prusa suggests the draft shield setting in the slicer, found under skirt and brim, to mitigate warping. The enclosure has a catch of its own: Prusa notes it can deform plastic printer parts inside it.
Fumes are the other half of the safety note. Prusa says ABS releases fumes that could pose a potential health risk. Print it in a well-ventilated room, and keep the room’s draught away from the print.
Acetone smoothing is what ABS gives you
Acetone vapour is a solvent that melts the surface of ABS glossy. Prusa says the surface “can be smoothed with acetone” to a glossy, smooth finish, and that the parts can also be sanded. ABS also glues together and paints well over a primer, so it suits parts that get finished after printing.
ABS yellows and turns brittle outdoors
Prusa warns that ABS parts used outdoors turn yellowish and more brittle over time, and describes its UV resistance as slightly worse than ASA’s. For anything in Singapore’s sun or rain, use ASA. ABS across its layers is also weak: it takes about a fifth of the knock it takes along them.
Acetone, glue and screw threads: ABS jobs at the studio
We print ABS in our own studio, and we pick it for warm indoor parts and car interiors, and for parts you want to smooth, glue or cut screw threads into. Because the layers are the weak direction, tell us how the part is loaded and we turn it so the load runs along them.
Acetone smoothing is not in the instant quote. Ask our team, and say whether the part will be painted afterwards, since our finishing service sands, primes and sprays. If the part will sit in full sun all day, we will likely suggest ASA.
Frequently asked
Does ABS need an enclosure?
Yes. Prusa lists a required printer enclosure as a drawback of ABS, because the part warps as it cools in open air. If you have no enclosure, Prusa suggests turning on the draft shield in the slicer, which reduces warping but does not remove it.
Is ABS or ASA better?
ASA is better for anything in the sun and softens a little later (about 90°C against 85°C). ABS suits indoor parts and parts you want to smooth with acetone. Both sand, prime and paint well.
Are ABS fumes dangerous?
Print ABS in a well-ventilated room. Prusa warns that it releases fumes that could pose a health risk, and names styrene. Ventilate the room without creating a draught around the print.
Related terms
Read next
Mentioned in
- 3D printer enclosure
- Acetone smoothing
- Annealing
- ASA filament
- Bakelite
- Bridging (3D printing)
- CNC router
- CO2 laser
- Fibreglass
- Living hinge
- Nylon filament
- PLA filament
- Polypropylene
- Polyurethane resin
- PTFE (Teflon)
- PU leather
- Thermoplastic
- Warping (3D printing)
- White ink
- What is a 3D pen, and is it the same as a 3D printer?
- How much does 3D printing cost in Singapore?
- How much clearance do 3D printed parts need to fit together?
- One part, 50 or 5,000: 3D printing, silicone moulding or injection moulding?
- What is a 3DBenchy, and what do the flaws on your boat mean?