Bridging in 3D printing
Printing layers across thin air between two supported points with no support underneath, which only works well over short distances.
Bridging is printing layers over thin air without supports. Prusa defines it that way, and notes that the best results come only over short distances. The plastic has to cool mid-air to make a solid link, and the printer’s fans do that job.
A bridge spans two supported points. That is the difference from an overhang, which leans out from one side only. The typical failure is sagging or drooping.
How far a filament bridge can span
How far a bridge can go depends on the printer, the material and the cooling. These figures are a conservative guide for filament:
| Material | Span for a clean underside |
|---|---|
| PLA | Under about 10 mm |
| PETG, ABS, ASA | Nearer 5 mm |
| Any filament, over 20 mm | Add a column or rib, or use supports |
Between 10 and 20 mm in PLA usually prints, but the underside turns rough and may droop. PETG bridges less well than PLA, and the tougher filaments are all in the 5 mm group.
Slicer settings that stop a bridge sagging
Prusa names three: slicer settings, speed and cooling. Print bridges slowly and with a lower bridge flow, which means less plastic on the first bridging layer. The idea is to pull the string of plastic behind the nozzle so it drops less. Prusa suggests printing a bridging test model several times in the slicer, each with a different flow, to find the right value without many test prints.
Slicers also have a thick bridges option. Prusa says the old way, which printed bridges with extremely thick lines, reached longer distances but looked worse. The newer default uses your layer height, so it is reliable over shorter spans and looks much better.
Changing the model so a bridge is shorter or gone
Prusa’s best fix is to turn the part until the bridges disappear. Failing that, a support under the middle of a long bridge splits it in two. In the model, a chamfer can shorten bridging distances. A rib or column halfway does the same job and stays in the part.
What to do with a 20 mm span before you upload
Long bridges are one of six filament defects that start in the file. Over 20 mm in any filament, our guide says to add a column or a rib, or let us support it. Turning the part so the span prints standing up removes the bridge, as long as the load still runs along the layers. If a long span cannot change, say so in the quote notes. The figures above are for filament only, so ask us about a long span in another process.
Frequently asked
How long can a 3D printed bridge be?
It depends on the printer, the material and the cooling. As a conservative guide on filament, keep a span under about 10 mm in PLA and nearer 5 mm in PETG, ABS or ASA. Past 20 mm, add a column or a rib.
Why does my 3D print sag over a gap?
The plastic is laid in mid-air with nothing below it, and it droops before it cools. Prusa lists sagging as the typical bridging problem, and says the printer's fans need to cool the plastic mid-air to make a solid connection.
Is a bridge the same as an overhang?
No. An overhang leans out from one side. A bridge spans between two points that are both held up.