Additive Inn
Get instant quote

Nylon filament

Polyamide on a spool for filament printers: wear-resistant and tough, but it absorbs water from the air and warps as it cools.

3D printing Checked

Nylon filament is polyamide (PA) wound on a spool for filament printers. It resists wear, slides with low friction and is tough in thick sections. It is also one of the hardest filaments to print well, because it soaks up water from the air and warps as it cools.

Why nylon filament bubbles in humid air

Polyamide is hygroscopic: it pulls water out of the air. Prusa says a badly stored spool can absorb water weighing up to 10% of the filament’s weight. Moist filament makes bubbles, which leads to uneven layers and an ugly surface.

Prusa’s fix is to dry it before printing, at least 4 hours at a temperature below 90°C, and to keep it airtight with desiccant. It also lists polyamide among the filaments that need drying more often than PLA. A 65°C dryer is too cool for the job; nylon needs a dryer that reaches 80 to 90°C. Singapore’s air averages about 82% humidity, so an opened spool does not stay dry for long.

Nylon print settings: 285°C, a hot bed and a closed box

SettingPure polyamide (Prusa)
Nozzle temperature285°C
Bed temperature110°C
Build surfaceSpecial PA nylon sheet
EnclosureHelps a lot against warping
VentilationRequired: strong odour and ultrafine particles

Prusa says the settings are usually quite similar to polycarbonate. That is far hotter than the 210°C Prusa gives for PLA. An enclosed printer holds the warm air that stops the corners lifting, the same job it does for ABS.

Plain nylon, carbon-fibre nylon or nylon powder

Filling the nylon with carbon fibre changes the behaviour. Prusa says carbon-fibre nylons warp far less than plain ones and can be printed without an enclosure. These blends need a hardened-steel nozzle.

We print three carbon-fibre nylons in our own studio: PA6-CF, PAHT-CF and PPA-CF. The three differ most on water. PA6-CF takes up 2.35% of its weight and loses about a third of its stiffness when wet. PAHT-CF takes up 0.88%, so it is the pick for damp rooms. The engineering filament guide has the numbers.

Powder nylon is a different process, not a filament. A part that must flex, such as a clip or hinge, does better in nylon powder: it stretches 18 to 20% before breaking, against 5.8% for PA6-CF. For plain, unfilled nylon filament, ask us before you plan a job around it.

Frequently asked

Is nylon filament hard to print?

Yes. Prusa calls pure polyamide very hard to print and recommends it for experienced users only. It needs a nozzle near 285°C, a bed near 110°C, dry filament and a warm enclosure.

How do you dry nylon filament?

Prusa says to dry it before printing for at least 4 hours at a temperature below 90°C. The 65°C dryers sold for PLA and PETG are too cool, so use a dryer that reaches 80 to 90°C.

Does nylon filament warp?

Yes. Prusa names warping as the main disadvantage of pure polyamide, and a warm enclosure helps a lot. Carbon-fibre filled nylons warp far less and can be printed without one.

Chat with us