Warping in 3D printing
When the corners or edges of a 3D print curl up off the build plate because the plastic shrinks as it cools.
Warping is when the corners or edges of a 3D print curl up off the build plate while it prints, or when the finished part comes out bent. Prusa traces it to a sudden temperature difference between the hot nozzle and the cooler air around the part: “the plastic will shrink and warp”. A big flat area shrinks the most, so wide, thin bases lift first.
Which filaments lift their corners
| Filament | What Prusa and our guides say |
|---|---|
| PLA | Rarely warps on a clean plate |
| PETG | Needs a lot of part cooling, so an enclosure does it no good |
| ABS, ASA | Most likely to lift on large objects, together with PC Blend |
High-temperature plastics need warm air around them. That is why ABS and ASA go in an enclosed printer, and PLA and PETG do not.
Fixes at the printer, in order
- Clean the plate. Prusa says to keep the surface free of grease and to wipe it with isopropyl alcohol of 90% or more.
- Add a brim. Prusa calls it “a good way how to increase the adhesion to the print surface”.
- Add a thin layer of glue stick on the cold plate. It helps grip and protects the plate.
- Stop the draughts. Prusa says “An open window or an AC unit nearby the printer will increase the occurrence of warps.” That matters in an air-conditioned Singapore room.
- Check the part cooling fan on PLA and PETG, which need a lot of it.
- Enclose the printer for ABS and ASA. A printed skirt as tall as the part also holds heat around it.
- Slow down. A lower print speed “may help a lot with high-warping materials”.
If a brim is not enough, Prusa suggests a tiny extra shape, a few layers tall, on the corner that keeps lifting.
Changing the model so a flat base stays down
You can often remove the problem in the model. Round the corners of a large flat base, split a very large flat part into pieces, and add a small chamfer to the bottom edge. The full list is in our guide to print defects you fix in the design.
Wide thin plates on a studio order
Someone at the studio reads each file and flags a base that is likely to warp. If you are sending a wide, thin plate that has to stay flat, say so in the quote notes, and ask us which process and material suit it.
Frequently asked
Why do my 3D prints lift at the corners?
The plastic cools and shrinks, and the shrinking pulls the corners up off the plate. It is worst on large flat parts and with high-temperature filaments such as ABS and ASA. A clean plate and a brim fix most cases.
Does PLA warp?
Rarely. PLA usually stays down on a clean plate, and ABS and ASA are the filaments that curl. If PLA lifts, wipe the plate with isopropyl alcohol, add a brim and check that the part cooling fan works.
Does an air conditioner cause warping?
It can. A cold draught on a part that is still cooling makes it shrink unevenly. Keep the printer away from the aircon outlet and open windows, or put it in an enclosure.