Additive Inn
Get instant quote

Stringing

Thin hairs of plastic left between the parts of a 3D print when the nozzle leaks while it travels.

3D printing Checked

Stringing is the thin hairs of plastic a filament printer leaves between the parts of a print. It happens when plastic keeps flowing out of the nozzle while the print head travels from one object or area to the next. It is also called oozing, or a “hairy” print.

Why damp filament strings the worst

Prusa says stringing is caused by “very high printing temperatures and/or using incorrect retraction settings”, and also that a spool that has “gathered moisture” will cause “a lot of stringing”. In Singapore, the moisture is the one to check first. Opened filament takes water from the air, and the water turns to steam in the hot nozzle.

Signs of a wet spool: popping at the nozzle, a rough or bubbly surface, and hairs everywhere. Prusa lists blobs, bubbling and smoke during extrusion too. Nylon, PVA and TPU need drying more often than PLA, and Prusa adds that “Some filaments are naturally more stringy than others.” Our filament dryer guide covers how to dry and store spools.

Settings that cut stringing

Work in this order and stop when the hairs go:

  1. Dry the spool, or try a different one.
  2. Lower the nozzle temperature by 5 to 10 °C.
  3. Check retraction in the slicer. This is the pull-back of filament before a travel move. Prusa warns that a larger minimum travel before retracting “will get lower printing times, but increase oozing and stringing”.
  4. Turn on avoid crossing perimeters, so the nozzle travels inside the part where hairs do not show.
  5. Clean the nozzle if you have printed one filament, such as PETG, for a long time.

Flexible filaments are a special case. Prusa notes they usually need longer retractions because they stretch.

Taking strings off a finished print

Prusa suggests a heat gun set to around 200 °C, aimed at the strings for one or two seconds. Longer than that “may deform the part”.

Dried spools on a studio order

The fixes above are spool and printer settings, so you do not need to change your model. The studio dries filament before printing. If strands show on a part you have received, ask us.

Frequently asked

Why does my 3D print have thin hairs between parts?

Plastic keeps leaking from the nozzle while it moves from one spot to the next. The usual causes are damp filament, a nozzle that is too hot and weak retraction settings.

How do I remove stringing from a finished print?

Hold a heat gun at about 200 degrees Celsius over the strings for one or two seconds, which melts them. Leave it longer and the part can deform.

Does Singapore's humidity cause stringing?

Often. Opened filament takes up water from humid air, and wet plastic strings badly. Dry the spool and store it sealed with desiccant before you touch any setting.