Overhang in 3D printing
A part of a 3D print that leans out past the layer below it, leaving little or nothing underneath for the plastic to rest on.
An overhang is any part of a model that leans out past the layer below it. A filament printer cannot print in mid-air: Prusa says each layer has to be laid on top of another one. Where a layer sticks out too far, the plastic has nothing to rest on and droops.
Steepness is measured from vertical. A straight wall is 0 degrees, and a flat shelf that sticks out of a wall is the extreme case. Our rule for filament files is overhangs within 45 degrees of vertical. Prusa puts the clean range at 45 to 60 degrees, depending on nozzle diameter and settings.
What a failed overhang looks like
Past the limit, the underside comes out rough and drooping. The usual fix is supports, which are thin scaffolding printed underneath. Supports leave marks when they come off, and Prusa notes that the surface above them looks worse than a side wall. A smaller nozzle, such as 0.25 mm, can bring the safe angle below 45 degrees.
Finer layers let a slightly steeper overhang print cleanly, at the cost of print time.
Three model changes that remove an overhang
| Change in the model | Why it works |
|---|---|
| 45 degree chamfer under a ledge | Each layer sits on the one below, so the ledge holds itself up |
| Turn the part | A steep face that points up or sideways needs nothing under it |
| Split the part and glue it | Each piece prints in a better orientation |
A rounded fillet is no substitute for the chamfer. Prusa says a fillet facing the bed makes a very steep overhang, so choose a chamfer when the finish matters. Where a support cannot be avoided, put it on a face nobody will see.
An overhang is also not a bridge. A bridge spans two held-up points, and an overhang leans out from one side.
Which faces of a metal print need to stay clean
The angle limit moves with the material. For metal parts we stand the part so faces that show are within 45 degrees of vertical, or 35 degrees for 316L stainless steel, and put supports on the faces you will not see. Tell us which faces must stay clean. On filament, overhangs within 45 degrees of vertical is one of four rules that catch most problems, so a flat ledge in the file is worth a note in the quote. If you only have a sketch or a sample, our design service can build the model for you.
Frequently asked
What angle can a 3D printer print without supports?
Prusa says a printer can cleanly print overhangs at an angle between 45 and 60 degrees, depending on nozzle diameter and settings. Our filament rule is within 45 degrees of vertical.
Why does the underside of my 3D print look rough?
Plastic laid over empty space has nothing to rest on, so it droops. If supports were used, the surface above them also looks worse than a side wall, because the supports leave a gap and marks.
How do I avoid overhangs in a 3D model?
Put a 45 degree chamfer under ledges instead of a flat shelf, turn the part so the steep face points up or sideways, or split it into pieces that print in a better orientation and glue them together.