Draft angle

A slight taper on the walls of a moulded or cast part, measured in degrees, so the part slides out of the mould instead of gripping it.

Designing parts Checked

A draft angle is the amount of taper on the walls of a moulded or cast part, measured in degrees. It is taken perpendicular to the parting line, the line where the mould halves meet. The taper lets the part slide out of the mould instead of gripping it.

Wikipedia’s example is a hollow plastic box with no lid. Once the plastic hardens around the mould, the mould has to come out, and the plastic may contract slightly as it hardens. Tapering the mould’s sides by 2 degrees, for instance, makes the mould easier to remove.

Draft figures from 1 degree to 12

SituationDraftSource
General rule1 degree per 1 inch (25 mm) of cavity depthProtolabs
Light texture1 to 5 degreesProtolabs Network
Leather or snakeskin texture5 to 12 degrees or moreProtolabs Network
Vacuum forming, raised (male) mouldabout 4 to 5 degreesFormlabs, quoted in our guide
Vacuum forming, hollow (female) mould1.5 to 3 degreesFormlabs, quoted in our guide

Protolabs says no single draft angle suits every part. Wall thickness, material, ejection method, shrink rate, finish and wall depth all change the number. Protolabs Network adds that the more a plastic shrinks, the more draft it needs.

What a part with no draft does to the mould

Without enough draft, parts risk drag marks and poor surface finish, and may bend, crack or warp from cooling stresses. Protolabs Network says a part with no taper comes out scratched and the mould wears. In severe cases the part cannot be ejected and the mould itself is damaged.

Why a printed prototype hides the problem

A 3D printed or machined prototype does not need draft, so it is often left out. Protolabs advises adding it from the start if the design may move to injection moulding, because draft changes how parts fit together and how they look. Designing it in early helps avoid costly redesigns.

What we say about draft in silicone, forming and tooling

Our silicone moulding page warns that parts with zero draft or sharp internal corners tear the silicone when demoulding. Our vacuum casting guide says straight walls with no taper grip the silicone as the part comes out, which wears or tears the mould. For vacuum forming we quote about 4 to 5 degrees on a raised mould and 1.5 to 3 degrees on a hollow one, more for deep or textured shapes, citing Formlabs.

For injection moulding, our design review adds draft angles and fixes undercuts before any tool steel is cut. Send your file and say which process it is for.

Frequently asked

What is a good draft angle?

Protolabs gives a rule of thumb of 1 degree of draft for every 1 inch (25 mm) of cavity depth, and says no single angle suits every part. Texture, material and wall depth change it.

Does a 3D printed part need draft?

A printed part does not need draft to be printed, but Protolabs advises adding it from the start if the design will move to injection moulding. Adding it later can change form and fit.

How much draft does a textured surface need?

Protolabs Network says a light texture suits 1 to 5 degrees of draft, and complex textures like leather or snakeskin need 5 to 12 degrees or more.

What happens if a part has no draft?

Protolabs says parts risk drag marks and poor surface finish, and may bend, crack or warp. In severe cases the part cannot be ejected cleanly and the mould can be damaged.